Effect of feldspar porcelain coating upon the wear ...
2013-1-15 · The wear tests were carried out in-vitro in linear reciprocating sliding mode. Pin-on-plate test geometry (prototype, Fig. 1) was used, with human molar cusps as pins and plates of veneered and unveneered commercial zirconia.Before and after testing the pins were placed in an oven during 48 h at 35 °C, to guarantee the same level of hydration during weighing.
Get Price